Density Reference Article
Density Name Symbol #
0.0899 g/L Hydrogen H 1
0.1785 g/L Helium He 2
0.9 g/L Neon Ne 10
1.2506 g/L Nitrogen N 7
1.429 g/L Oxygen O 8
1.696 g/L Fluorine F 9
1.7824 g/L Argon Ar 18
3.214 g/L Chlorine Cl 17
3.75 g/L Krypton Kr 36
5.9 g/L Xenon Xe 54
9.73 g/L Radon Rn 86
0.534 g/cc Lithium Li 3
0.862 g/cc Potassium K 19
0.971 g/cc Sodium Na 11
1.55 g/cc Calcium Ca 20
1.63 g/cc Rubidium Rb 37
1.738 g/cc Magnesium Mg 12
1.82 g/cc Phosphorus P 15
1.848 g/cc Beryllium Be 4
1.873 g/cc Cesium Cs 55
2.07 g/cc Sulfur S 16
2.26 g/cc Carbon C 6
2.33 g/cc Silicon Si 14
2.34 g/cc Boron B 5
2.54 g/cc Strontium Sr 38
2.702 g/cc Aluminum Al 13
2.99 g/cc Scandium Sc 21
3.119 g/cc Bromine Br 35
3.59 g/cc Barium Ba 56
4.47 g/cc Yttrium Y 39
4.54 g/cc Titanium Ti 22
4.79 g/cc Selenium Se 34
4.93 g/cc Iodine I 53
5.24 g/cc Europium Eu 63
5.323 g/cc Germanium Ge 32
5.5 g/cc Radium Ra 88
5.72 g/cc Arsenic As 33
5.907 g/cc Gallium Ga 31
6.11 g/cc Vanadium V 23
6.15 g/cc Lanthanum La 57
6.24 g/cc Tellurium Te 52
6.51 g/cc Zirconium Zr 40
6.684 g/cc Antimony Sb 51
6.77 g/cc Praseodymium Pr 59
6.77 g/cc Cerium Ce 58
6.9 g/cc Ytterbium Yb 70
7.01 g/cc Neodymium Nd 60
7.13 g/cc Zinc Zn 30
7.19 g/cc Chromium Cr 24
7.3 g/cc Promethium Pm 61
7.31 g/cc Indium In 49
7.31 g/cc Tin Sn 50
7.43 g/cc Manganese Mn 25
7.52 g/cc Samarium Sm 62
7.874 g/cc Iron Fe 26
7.895 g/cc Gadolinium Gd 64
8.23 g/cc Terbium Tb 65
8.55 g/cc Dysprosium Dy 66
8.57 g/cc Niobium Nb 41
8.65 g/cc Cadmium Cd 48
8.8 g/cc Holmium Ho 67
8.9 g/cc Cobalt Co 27
8.9 g/cc Nickel Ni 28
8.96 g/cc Copper Cu 29
9.07 g/cc Erbium Er 68
9.3 g/cc Polonium Po 84
9.32 g/cc Thulium Tm 69
9.75 g/cc Bismuth Bi 83
9.84 g/cc Lutetium Lu 71
10.07 g/cc Actinium Ac 89
10.22 g/cc Molybdenum Mo 42
10.5 g/cc Silver Ag 47
11.35 g/cc Lead Pb 82
11.5 g/cc Technetium Tc 43
11.724 g/cc Thorium Th 90
11.85 g/cc Thallium Tl 81
12.02 g/cc Palladium Pd 46
12.37 g/cc Ruthenium Ru 44
12.41 g/cc Rhodium Rh 45
13.31 g/cc Hafnium Hf 72
13.5 g/cc Curium Cm 96
13.546 g/cc Mercury Hg 80
13.67 g/cc Americium Am 95
14.78 g/cc Berkelium Bk 97
15.1 g/cc Californium Cf 98
15.4 g/cc Protactinium Pa 91
16.65 g/cc Tantalum Ta 73
18.95 g/cc Uranium U 92
19.32 g/cc Gold Au 79
19.35 g/cc Tungsten W 74
19.84 g/cc Plutonium Pu 94
20.2 g/cc Neptunium Np 93
21.04 g/cc Rhenium Re 75
21.45 g/cc Platinum Pt 78
22.4 g/cc Iridium Ir 77
22.6 g/cc Osmium Os 76