Electrical Conductivity Reference |
| Electrical Conductivity |
Name |
Symbol |
# |
| 5.0E-24 106/cm Ω |
Sulfur |
S |
16 |
| 1.0E-17 106/cm Ω |
Phosphorus |
P |
15 |
| 8.0E-16 106/cm Ω |
Iodine |
I |
53 |
| 1.0E-12 106/cm Ω |
Selenium |
Se |
34 |
| 1.0E-12 106/cm Ω |
Boron |
B |
5 |
| 2.52E-12 106/cm Ω |
Silicon |
Si |
14 |
| 1.45E-8 106/cm Ω |
Geranium |
Ge |
32 |
| 2.0E-6 106/cm Ω |
Tellurium |
Te |
52 |
| 0.00061 106/cm Ω |
Carbon |
C |
6 |
| 0.00666 106/cm Ω |
Plutonium |
Pu |
94 |
| 0.00695 106/cm Ω |
Manganese |
Mn |
25 |
| 0.00736 106/cm Ω |
Gadolinium |
Gd |
64 |
| 0.00822 106/cm Ω |
Neptunium |
Np |
93 |
| 0.00867 106/cm Ω |
Bismuth |
Bi |
83 |
| 0.00889 106/cm Ω |
Terbium |
Tb |
65 |
| 0.00956 106/cm Ω |
Samarium |
Sm |
62 |
| 0.0104 106/cm Ω |
Mercury |
Hg |
80 |
| 0.0108 106/cm Ω |
Dysprosium |
Dy |
66 |
| 0.0112 106/cm Ω |
Europium |
Eu |
63 |
| 0.0115 106/cm Ω |
Cerium |
Ce |
58 |
| 0.0117 106/cm Ω |
Erbium |
Er |
68 |
| 0.0124 106/cm Ω |
Holmium |
Ho |
67 |
| 0.0126 106/cm Ω |
Lanthanum |
La |
57 |
| 0.0148 106/cm Ω |
Praseodymium |
Pr |
59 |
| 0.015 106/cm Ω |
Thulium |
Tm |
69 |
| 0.0157 106/cm Ω |
Neodymium |
Nd |
60 |
| 0.0166 106/cm Ω |
Yttrium |
Y |
39 |
| 0.0177 106/cm Ω |
Scandium |
Sc |
21 |
| 0.0185 106/cm Ω |
Lutetium |
Lu |
71 |
| 0.0219 106/cm Ω |
Polonium |
Po |
84 |
| 0.022 106/cm Ω |
Americium |
Am |
95 |
| 0.0234 106/cm Ω |
Titanium |
Ti |
22 |
| 0.0236 106/cm Ω |
Zirconium |
Zr |
40 |
| 0.0288 106/cm Ω |
Antimony |
Sb |
51 |
| 0.03 106/cm Ω |
Francium |
Fr |
87 |
| 0.03 106/cm Ω |
Barium |
Ba |
56 |
| 0.0312 106/cm Ω |
Hafnium |
Hf |
72 |
| 0.0345 106/cm Ω |
Arsenic |
As |
33 |
| 0.0351 106/cm Ω |
Ytterbium |
Yb |
70 |
| 0.038 106/cm Ω |
Uranium |
U |
92 |
| 0.0481 106/cm Ω |
Lead |
Pb |
82 |
| 0.0489 106/cm Ω |
Vanadium |
V |
23 |
| 0.0489 106/cm Ω |
Cesium |
Cs |
55 |
| 0.0529 106/cm Ω |
Protactinium |
Pa |
91 |
| 0.0542 106/cm Ω |
Rhenium |
Re |
75 |
| 0.0617 106/cm Ω |
Thallium |
Tl |
81 |
| 0.0653 106/cm Ω |
Thorium |
Th |
90 |
| 0.067 106/cm Ω |
Technetium |
Tc |
43 |
| 0.0678 106/cm Ω |
Gallium |
Ga |
31 |
| 0.0693 106/cm Ω |
Niobium |
Nb |
41 |
| 0.0761 106/cm Ω |
Tantalum |
Ta |
73 |
| 0.0762 106/cm Ω |
Strontium |
Sr |
38 |
| 0.0774 106/cm Ω |
Chromium |
Cr |
24 |
| 0.0779 106/cm Ω |
Rubidium |
Rb |
37 |
| 0.0917 106/cm Ω |
Tin |
Sn |
50 |
| 0.095 106/cm Ω |
Palladium |
Pd |
46 |
| 0.0966 106/cm Ω |
Platinum |
Pt |
78 |
| 0.0993 106/cm Ω |
Iron |
Fe |
26 |
| 0.108 106/cm Ω |
Lithium |
Li |
3 |
| 0.109 106/cm Ω |
Osmium |
Os |
76 |
| 0.116 106/cm Ω |
Indium |
In |
49 |
| 0.137 106/cm Ω |
Ruthenium |
Ru |
44 |
| 0.138 106/cm Ω |
Cadmium |
Cd |
48 |
| 0.139 106/cm Ω |
Potassium |
K |
19 |
| 0.143 106/cm Ω |
Nickel |
Ni |
28 |
| 0.166 106/cm Ω |
Zinc |
Zn |
30 |
| 0.172 106/cm Ω |
Cobalt |
Co |
27 |
| 0.187 106/cm Ω |
Molybdenum |
Mo |
42 |
| 0.189 106/cm Ω |
Tungsten |
W |
74 |
| 0.197 106/cm Ω |
Iridium |
Ir |
77 |
| 0.21 106/cm Ω |
Sodium |
Na |
11 |
| 0.211 106/cm Ω |
Rhodium |
Rh |
45 |
| 0.226 106/cm Ω |
Magnesium |
Mg |
12 |
| 0.298 106/cm Ω |
Calcium |
Ca |
20 |
| 0.313 106/cm Ω |
Beryllium |
Be |
4 |
| 0.377 106/cm Ω |
Aluminum |
Al |
13 |
| 0.452 106/cm Ω |
Gold |
Au |
79 |
| 0.596 106/cm Ω |
Copper |
Cu |
29 |
| 0.63 106/cm Ω |
Silver |
Ag |
47 |
|