0.95 K -272.05 °C -458 °F Helium He 2
14.025 K -258.975 °C -434 °F Hydrogen H 1
24.553 K -248.447 °C -415.205 °F Neon Ne 10
50.35 K -222.65 °C -368.77 °F Oxygen O 8
53.48 K -219.52 °C -363.14 °F Fluorine F 9
63.14 K -209.86 °C -345.75 °F Nitrogen N 7
83.81 K -189.19 °C -308.54 °F Argon Ar 18
115.78 K -157.22 °C -251 °F Krypton Kr 36
161.3 K -111.7 °C -169.1 °F Xenon Xe 54
172.16 K -100.84 °C -149.51 °F Chlorine Cl 17
202 K -71 °C -96 °F Radon Rn 86
234.28 K -38.72 °C -37.7 °F Mercury Hg 80
265.9 K -7.1 °C 19.2 °F Bromine Br 35
300 K 27 °C 81 °F Francium Fr 87
301.55 K 28.55 °C 83.39 °F Cesium Cs 55
302.9 K 29.9 °C 85.8 °F Gallium Ga 31
312.64 K 39.64 °C 103.35 °F Rubidium Rb 37
317.3 K 44.3 °C 111.7 °F Phosphorus P 15
336.35 K 63.35 °C 146.03 °F Potassium K 19
371 K 98 °C 208 °F Sodium Na 11
386.7 K 113.5 °C 236.3 °F Iodine I 53
388.36 K 115.36 °C 239.65 °F Sulfur S 16
429.76 K 156.76 °C 314.17 °F Indium In 49
453.7 K 180.7 °C 357.3 °F Lithium Li 3
494 K 221 °C 430 °F Selenium Se 34
505.06 K 232.06 °C 449.71 °F Tin Sn 50
527 K 254 °C 489 °F Polonium Po 84
544.52 K 271.52 °C 520.74 °F Bismuth Bi 83
575 K 302 °C 576 °F Astatine At 85
577 K 304 °C 579 °F Thallium Tl 81
594.18 K 321.18 °C 610.12 °F Cadmium Cd 48
600.6 K 327.6 °C 621.7 °F Lead Pb 82
692.73 K 419.73 °C 787.51 °F Zinc Zn 30
722.65 K 449.65 °C 841.37 °F Tellurium Te 52
903.9 K 630.9 °C 1167.6 °F Antimony Sb 51
913 K 640 °C 1184 °F Plutonium Pu 94
913 K 640 °C 1184 °F Neptunium Np 93
922 K 649 °C 1200 °F Magnesium Mg 12
933.25 K 660.25 °C 1220.45 °F Aluminum Al 13
973 K 700 °C 1292 °F Radium Ra 88
1002 K 729 °C 1344 °F Barium Ba 56
1042 K 769 °C 1416 °F Strontium Sr 38
1071 K 798 °C 1468 °F Cerium Ce 58
1081 K 808 °C 1486 °F Arsenic As 33
1095 K 822 °C 1512 °F Europium Eu 63
1097 K 824 °C 1515 °F Ytterbium Yb 70
1112 K 839 °C 1542 °F Calcium Ca 20
1133 K 860 °C 1580 °F Einsteinium Es 99
1173 K 900 °C 1652 °F Californium Cf 98
1193 K 920 °C 1688 °F Lanthanum La 57
1204 K 931 °C 1708 °F Promethium Pm 61
1204 K 931 °C 1708 °F Praseodymium Pr 59
1210.4 K 937.4 °C 1719.3 °F Germanium Ge 32
1234 K 961 °C 1762 °F Silver Ag 47
1259 K 986 °C 1807 °F Berkelium B K 97
1267 K 994 °C 1821 °F Americium Am 95
1289 K 1016 °C 1861 °F Neodymium Nd 60
1323 K 1050 °C 1922 °F Actinium Ac 89
1337.58 K 1064.58 °C 1948.24 °F Gold Au 79
1340 K 1067 °C 1953 °F Curium Cm 96
1345 K 1072 °C 1962 °F Samarium Sm 62
1357.6 K 1084.6 °C 1984.3 °F Copper Cu 29
1405 K 1132 °C 2070 °F Uranium U 92
1517 K 1244 °C 2271 °F Manganese Mn 25
1551 K 1278 °C 2332 °F Beryllium Be 4
1585 K 1312 °C 2394 °F Gadolinium Gd 64
1630 K 1357 °C 2475 °F Terbium Tb 65
1683 K 1410 °C 2570 °F Silicon Si 14
1685 K 1412 °C 2574 °F Dysprosium Dy 66
1726 K 1453 °C 2647 °F Nickel Ni 28
1743 K 1470 °C 2678 °F Holmium Ho 67
1768 K 1495 °C 2723 °F Cobalt Co 27
1795 K 1522 °C 2772 °F Erbium Er 68
1799 K 1526 °C 2779 °F Yttrium Y 39
1808 K 1535 °C 2795 °F Iron Fe 26
1812 K 1539 °C 2802 °F Scandium Sc 21
1818 K 1545 °C 2813 °F Thulium Tm 69
1825 K 1552 °C 2826 °F Palladium Pd 46
1933 K 1660 °C 3020 °F Titanium Ti 22
1936 K 1663 °C 3025 °F Lutetium Lu 71
2028 K 1755 °C 3191 °F Thorium Th 90
2045 K 1772 °C 3222 °F Platinum Pt 78
2113 K 1600 °C 2912 °F Protactinium Pa 91
2125 K 1852 °C 3366 °F Zirconium Zr 40
2130 K 1857 °C 3375 °F Chromium Cr 24
2175 K 1902 °C 3456 °F Vanadium V 23
2239 K 1966 °C 3571 °F Rhodium Rh 45
2473 K 2200 °C 3992 °F Technetium Tc 43
2500 K 2227 °C 4041 °F Hafnium HF 72
2523 K 2250 °C 4082 °F Ruthenium Ru 44
2573 K 2300 °C 4172 °F Boron B 5
2716 K 2443 °C 4429 °F Iridium Ir 77
2741 K 2468 °C 4474 °F Niobium Nb 41
2890 K 2617 °C 4743 °F Molybdenum Mo 42
3269 K 2996 °C 5425 °F Tantalum Ta 73
3300 K 3027 °C 5481 °F Osmium Os 76
3453 K 3180 °C 5756 °F Rhenium Re 75
3680 K 3407 °C 6165 °F Tungsten W 74
3773 K 3500 °C 6332 °F Carbon C 6