Thermal Conductivity Reference
Thermal Conductivity Name Symbol #
0.0000364 W/cmK Radon Rn 86
0.0000569 W/cmK Xenon Xe 54
0.000089 W/cmK Chlorine Cl 17
0.0000949 W/cmK Krypton Kr 36
0.0001772 W/cmK Argon Ar 18
0.0002598 W/cmK Nitrogen N 7
0.0002674 W/cmK Oxygen O 8
0.000279 W/cmK Fluorine F 9
0.000493 W/cmK Neon Ne 10
0.00122 W/cmK Bromine Br 35
0.00152 W/cmK Helium He 2
0.001815 W/cmK Hydrogen H 1
0.00235 W/cmK Phosphorus P 15
0.00269 W/cmK Sulfur S 16
0.00449 W/cmK Iodine I 53
0.017 W/cmK Astatine At 85
0.0204 W/cmK Selenium Se 34
0.0235 W/cmK Tellurium Te 52
0.063 W/cmK Neptunium Np 93
0.0674 W/cmK Plutonium Pu 94
0.0782 W/cmK Manganese Mn 25
0.0787 W/cmK Bismuth Bi 83
0.0834 W/cmK Mercury Hg 80
0.1 W/cmK Americium Am 95
0.1 W/cmK Californium Cf 98
0.1 W/cmK Nobelium No 102
0.1 W/cmK Curium Cm 96
0.1 W/cmK Lawrencium Lr 103
0.1 W/cmK Fermium Fm 100
0.1 W/cmK Einsteinium Es 99
0.1 W/cmK Berkelium Bk 97
0.1 W/cmK Mendelevium Md 101
0.106 W/cmK Gadolinium Gd 64
0.107 W/cmK Dysprosium Dy 66
0.111 W/cmK Terbium Tb 65
0.114 W/cmK Cerium Ce 58
0.12 W/cmK Actinium Ac 89
0.125 W/cmK Praseodymium Pr 59
0.133 W/cmK Samarium Sm 62
0.135 W/cmK Lanthanum La 57
0.139 W/cmK Europium Eu 63
0.143 W/cmK Erbium Er 68
0.15 W/cmK Francium Fr 87
0.158 W/cmK Scandium Sc 21
0.162 W/cmK Holmium Ho 67
0.164 W/cmK Lutetium Lu 71
0.165 W/cmK Neodymium Nd 60
0.168 W/cmK Thulium Tm 69
0.172 W/cmK Yttrium Y 39
0.179 W/cmK Promethium Pm 61
0.184 W/cmK Barium Ba 56
0.186 W/cmK Radium Ra 88
0.2 W/cmK Polonium Po 84
0.219 W/cmK Titanium Ti 22
0.227 W/cmK Zirconium Zr 40
0.23 W/cmK Hafnium Hf 72
0.23 W/cmK Rutherfordium Rf 104
0.243 W/cmK Antimony Sb 51
0.274 W/cmK Boron B 5
0.276 W/cmK Uranium U 92
0.307 W/cmK Vanadium V 23
0.349 W/cmK Ytterbium Yb 70
0.353 W/cmK Strontium Sr 38
0.353 W/cmK Lead Pb 82
0.359 W/cmK Cesium Cs 55
0.406 W/cmK Gallium Ga 31
0.461 W/cmK Thallium Tl 81
0.47 W/cmK Protactinium Pa 91
0.479 W/cmK Rhenium Re 75
0.502 W/cmK Arsenic As 33
0.506 W/cmK Technetium Tc 43
0.537 W/cmK Niobium Nb 41
0.54 W/cmK Thorium Th 90
0.575 W/cmK Tantalum Ta 73
0.58 W/cmK Dubnium Db 105
0.582 W/cmK Rubidium Rb 37
0.599 W/cmK Germanium Ge 32
0.666 W/cmK Tin Sn 50
0.716 W/cmK Platinum Pt 78
0.718 W/cmK Palladium Pd 46
0.802 W/cmK Iron Fe 26
0.816 W/cmK Indium In 49
0.847 W/cmK Lithium Li 3
0.876 W/cmK Osmium Os 76
0.907 W/cmK Nickel Ni 28
0.937 W/cmK Chromium Cr 24
0.968 W/cmK Cadmium Cd 48
1 W/cmK Cobalt Co 27
1.024 W/cmK Potassium K 19
1.16 W/cmK Zinc Zn 30
1.17 W/cmK Ruthenium Ru 44
1.29 W/cmK Carbon C 6
1.38 W/cmK Molybdenum Mo 42
1.41 W/cmK Sodium Na 11
1.47 W/cmK Iridium Ir 77
1.48 W/cmK Silicon Si 14
1.5 W/cmK Rhodium Rh 45
1.56 W/cmK Magnesium Mg 12
1.74 W/cmK Tungsten W 74
2.01 W/cmK Calcium Ca 20
2.01 W/cmK Beryllium Be 4
2.37 W/cmK Aluminum Al 13
3.17 W/cmK Gold Au 79
4.01 W/cmK Copper Cu 29
4.29 W/cmK Silver Ag 47