# What is DC Sputtering?

- **URL:** https://www.semicore.com/news/94-what-is-dc-sputtering
- **Published:** 2016-11-26

DC (Direct Current) Sputtering is a Thin Film Physical Vapor Deposition (PVD) Coating technique where a target material to be used as the coating is bombarded with ionized gas molecules causing atoms to be “Sputtered” off into the plasma. These vaporized atoms are then deposited and condense as a thin film on the substrate to be coated. Diagram of the DC Magnetron Sputtering Process DC Sputtering is the most basic and inexpensive type of sputtering system for PVD based metal deposition and electrically conductive target coating materials. Two major advantages of DC as a power source for this process is that it is easy to control and is a low-cost option if you are doing metal deposition for coating. DC Sputtering is used extensively in the semiconductor industry for creating microchip circuitry on the molecular level. It is used for gold sputter coatings of jewelry, watches and other decorative finishes, and may be found in processes for non-reflective coatings on glass and optical components, as well as for metalized packaging plastics. There are several key factors to the basic configuration of a DC Sputtering based coating system. First, the target material to be used as a coating is to be placed in a vacuum chamber parallel to the substrate to be coated most commonly, though other methods can be used. The vacuum chamber is then evacuated to a base pressure. Typical sputtering ranges are between 0.5mTorr to 100mTorr, removing H2O, Air, N2, and other contaminants. Then, the chamber is backfilled with a high purity, inert, process gas – usually Argon due to its relative mass and ability to convey kinetic energy upon impact. This occurs during high energy molecular collisions in the plasma in order to create the gas ions that are the primary driving force of sputter-based thin film deposition. What is Sputtering? Video A DC electrical current typically in the -2 to -5 kV range is then applied to the target coating material that is the cathode or point at which electrons enter the system known as the negative bias. A positive charge is also applied to the substrate to be coated which become the anode. The electrically neutral argon gas atoms are first ionized as a result of the forceful collision of these gas atoms onto the surface of the negatively charged target, which eject atoms off into the plasma – a hot gas-like state consisting of roughly half gas ions and half electrons that emits a visible glow. The ionized argon gas atoms are then driven to the substrate, which is the anode or positive charged bias. This attracts ionized gas ions, electrons and the vaporized target coating atoms, that then condense and form a thin film coating on the substrate to be coated. DC Magnetron sputtering system uses magnets behind the negative cathode to trap electrons over the negatively charged target material so they are not free to bombard the substrate, allowing for faster deposition rates. The magnetic field generated forms a boundary “tunnel” which traps electrons near the surface of the target. That improves the efficiency of the gas ion formation. DC Magnetron Sputtering allows for higher current at lower gas pressure that achieves an even higher thin film deposition rate. Diagram of the DC Sputtering Process DC Sputtering Equipment FAQs Video While DC Sputtering is the economical solution of choice for many types of metal coatings, its primary limitation is that non-conducting dielectric insulating materials take on a charge over time. This will eventually result in any one of a variety of issues including arcing, which is the poisoning of the target material with a charge that can result in the complete cessation of sputtering. To overcome these limitations of DC Sputtering, several more complicated technologies have been developed such as RF (Radio Frequency) Sputtering, and HIPIMS (High-Power Impulse Magnetron Sputtering). RF Sputtering alternates the electrical charge at Radio Frequency so as to prevent a charge buildup on the target or coating material. HIPIMS utilizes a very high voltage, short duration burst of energy focused on the target coating material to generate a high-density plasma that results in a high degree of ionization of the coating material in the plasma. Despite the relative simplicity of DC Sputtering, it usually has somewhat low deposition rates compared to the more complicated HIPIMS which is the result of lower plasma densities and higher gas densities. However, the relative simplicity of the DC Power source compared to RF or HIPMIS power sources that require much more complicated configuration, cabling and higher energy costs continues to make DC Sputtering the low-cost solution for many types of vacuum metal deposition like gold sputtering and other electrically conductive coatings. Semicore’s CAPOS all-in-one PVD Sputtering or Thermal Evaporation System CAPOS-CT Multi-Chamber PVD Coating System Video Semicore’s breakthrough CAPOS thin film deposition system is the PVD Industry’s first cost effective “Open-platform” design, that is ideal for both precision R&D and batch production. Flexible enough that it can be used for either sputtering or evaporation coatings, this platform is also used for Semicore’s CAPOS-CT series, as a highly versatile “Cluster Tool” platform that can be configured with multiple Process Modules (PM) and cassette-to-cassette operation that speeds production cycles. Read more... For more detailed information on these units’ specifications please download the PDF. Matt Hughes is President of Semicore Equipment Inc, a leading worldwide supplier of sputtering equipment for the electronics, solar energy, optical, medical, military, automotive, and related high tech industries. Please let our helpful support staff answer any questions you have regarding “What is DC Sputtering?” and how to implement the best techniques and equipment for your specific Metal Deposition DC Sputtering Equipment needs by contacting us at sales@semicore.com or by calling 925-373-8201.   Related Articles What is RF Sputtering? RF Sputtering can be used for the coating of dielectric or insulative materials that can take on a charge that results in arcing in the vacuum chamber with convention DC Sputtering. However, RF Sputtering deposition rates are slower than DC Sputtering rates and have higher power costs and so is usually used on smaller substrates to be coated... Read More   What is Pulsed DC Sputtering? Compared to conventional DC Sputtering, arcing can be greatly decreased or even eliminated by pulsing the DC voltage in the 10–350?kHz range with duty cycles in the 50–90% range.  A Pulsed DC electrical current typically in the few hundreds of volts range is applied to the target coating material. the voltage is either turned off or more frequently reversed with a low voltage short duration cycle to "cleanse" the target of any charge buildup... Read More   Photo:  CC BY-SA  Sherrie Thai SEO Expert Optimization
