| 5.0E-24 106/cm Ω | Sulfur | S | 16 |
| 1.0E-17 106/cm Ω | Phosphorus | P | 15 |
| 8.0E-16 106/cm Ω | Iodine | I | 53 |
| 1.0E-12 106/cm Ω | Selenium | Se | 34 |
| 1.0E-12 106/cm Ω | Boron | B | 5 |
| 2.52E-12 106/cm Ω | Silicon | Si | 14 |
| 1.45E-8 106/cm Ω | Geranium | Ge | 32 |
| 2.0E-6 106/cm Ω | Tellurium | Te | 52 |
| 0.00061 106/cm Ω | Carbon | C | 6 |
| 0.00666 106/cm Ω | Plutonium | Pu | 94 |
| 0.00695 106/cm Ω | Manganese | Mn | 25 |
| 0.00736 106/cm Ω | Gadolinium | Gd | 64 |
| 0.00822 106/cm Ω | Neptunium | Np | 93 |
| 0.00867 106/cm Ω | Bismuth | Bi | 83 |
| 0.00889 106/cm Ω | Terbium | Tb | 65 |
| 0.00956 106/cm Ω | Samarium | Sm | 62 |
| 0.0104 106/cm Ω | Mercury | Hg | 80 |
| 0.0108 106/cm Ω | Dysprosium | Dy | 66 |
| 0.0112 106/cm Ω | Europium | Eu | 63 |
| 0.0115 106/cm Ω | Cerium | Ce | 58 |
| 0.0117 106/cm Ω | Erbium | Er | 68 |
| 0.0124 106/cm Ω | Holmium | Ho | 67 |
| 0.0126 106/cm Ω | Lanthanum | La | 57 |
| 0.0148 106/cm Ω | Praseodymium | Pr | 59 |
| 0.015 106/cm Ω | Thulium | Tm | 69 |
| 0.0157 106/cm Ω | Neodymium | Nd | 60 |
| 0.0166 106/cm Ω | Yttrium | Y | 39 |
| 0.0177 106/cm Ω | Scandium | Sc | 21 |
| 0.0185 106/cm Ω | Lutetium | Lu | 71 |
| 0.0219 106/cm Ω | Polonium | Po | 84 |
| 0.022 106/cm Ω | Americium | Am | 95 |
| 0.0234 106/cm Ω | Titanium | Ti | 22 |
| 0.0236 106/cm Ω | Zirconium | Zr | 40 |
| 0.0288 106/cm Ω | Antimony | Sb | 51 |
| 0.03 106/cm Ω | Francium | Fr | 87 |
| 0.03 106/cm Ω | Barium | Ba | 56 |
| 0.0312 106/cm Ω | Hafnium | Hf | 72 |
| 0.0345 106/cm Ω | Arsenic | As | 33 |
| 0.0351 106/cm Ω | Ytterbium | Yb | 70 |
| 0.038 106/cm Ω | Uranium | U | 92 |
| 0.0481 106/cm Ω | Lead | Pb | 82 |
| 0.0489 106/cm Ω | Vanadium | V | 23 |
| 0.0489 106/cm Ω | Cesium | Cs | 55 |
| 0.0529 106/cm Ω | Protactinium | Pa | 91 |
| 0.0542 106/cm Ω | Rhenium | Re | 75 |
| 0.0617 106/cm Ω | Thallium | Tl | 81 |
| 0.0653 106/cm Ω | Thorium | Th | 90 |
| 0.067 106/cm Ω | Technetium | Tc | 43 |
| 0.0678 106/cm Ω | Gallium | Ga | 31 |
| 0.0693 106/cm Ω | Niobium | Nb | 41 |
| 0.0761 106/cm Ω | Tantalum | Ta | 73 |
| 0.0762 106/cm Ω | Strontium | Sr | 38 |
| 0.0774 106/cm Ω | Chromium | Cr | 24 |
| 0.0779 106/cm Ω | Rubidium | Rb | 37 |
| 0.0917 106/cm Ω | Tin | Sn | 50 |
| 0.095 106/cm Ω | Palladium | Pd | 46 |
| 0.0966 106/cm Ω | Platinum | Pt | 78 |
| 0.0993 106/cm Ω | Iron | Fe | 26 |
| 0.108 106/cm Ω | Lithium | Li | 3 |
| 0.109 106/cm Ω | Osmium | Os | 76 |
| 0.116 106/cm Ω | Indium | In | 49 |
| 0.137 106/cm Ω | Ruthenium | Ru | 44 |
| 0.138 106/cm Ω | Cadmium | Cd | 48 |
| 0.139 106/cm Ω | Potassium | K | 19 |
| 0.143 106/cm Ω | Nickel | Ni | 28 |
| 0.166 106/cm Ω | Zinc | Zn | 30 |
| 0.172 106/cm Ω | Cobalt | Co | 27 |
| 0.187 106/cm Ω | Molybdenum | Mo | 42 |
| 0.189 106/cm Ω | Tungsten | W | 74 |
| 0.197 106/cm Ω | Iridium | Ir | 77 |
| 0.21 106/cm Ω | Sodium | Na | 11 |
| 0.211 106/cm Ω | Rhodium | Rh | 45 |
| 0.226 106/cm Ω | Magnesium | Mg | 12 |
| 0.298 106/cm Ω | Calcium | Ca | 20 |
| 0.313 106/cm Ω | Beryllium | Be | 4 |
| 0.377 106/cm Ω | Aluminum | Al | 13 |
| 0.452 106/cm Ω | Gold | Au | 79 |
| 0.596 106/cm Ω | Copper | Cu | 29 |
| 0.63 106/cm Ω | Silver | Ag | 47 |