Skip to content | Melting Point | | Name | Symbol | # |
|---|
| 0.95 K | -272.05 °C | -458 °F | Helium | He | 2 |
| 14.025 K | -258.975 °C | -434 °F | Hydrogen | H | 1 |
| 24.553 K | -248.447 °C | -415.205 °F | Neon | Ne | 10 |
| 50.35 K | -222.65 °C | -368.77 °F | Oxygen | O | 8 |
| 53.48 K | -219.52 °C | -363.14 °F | Fluorine | F | 9 |
| 63.14 K | -209.86 °C | -345.75 °F | Nitrogen | N | 7 |
| 83.81 K | -189.19 °C | -308.54 °F | Argon | Ar | 18 |
| 115.78 K | -157.22 °C | -251 °F | Krypton | Kr | 36 |
| 161.3 K | -111.7 °C | -169.1 °F | Xenon | Xe | 54 |
| 172.16 K | -100.84 °C | -149.51 °F | Chlorine | Cl | 17 |
| 202 K | -71 °C | -96 °F | Radon | Rn | 86 |
| 234.28 K | -38.72 °C | -37.7 °F | Mercury | Hg | 80 |
| 265.9 K | -7.1 °C | 19.2 °F | Bromine | Br | 35 |
| 300 K | 27 °C | 81 °F | Francium | Fr | 87 |
| 301.55 K | 28.55 °C | 83.39 °F | Cesium | Cs | 55 |
| 302.9 K | 29.9 °C | 85.8 °F | Gallium | Ga | 31 |
| 312.64 K | 39.64 °C | 103.35 °F | Rubidium | Rb | 37 |
| 317.3 K | 44.3 °C | 111.7 °F | Phosphorus | P | 15 |
| 336.35 K | 63.35 °C | 146.03 °F | Potassium | K | 19 |
| 371 K | 98 °C | 208 °F | Sodium | Na | 11 |
| 386.7 K | 113.5 °C | 236.3 °F | Iodine | I | 53 |
| 388.36 K | 115.36 °C | 239.65 °F | Sulfur | S | 16 |
| 429.76 K | 156.76 °C | 314.17 °F | Indium | In | 49 |
| 453.7 K | 180.7 °C | 357.3 °F | Lithium | Li | 3 |
| 494 K | 221 °C | 430 °F | Selenium | Se | 34 |
| 505.06 K | 232.06 °C | 449.71 °F | Tin | Sn | 50 |
| 527 K | 254 °C | 489 °F | Polonium | Po | 84 |
| 544.52 K | 271.52 °C | 520.74 °F | Bismuth | Bi | 83 |
| 575 K | 302 °C | 576 °F | Astatine | At | 85 |
| 577 K | 304 °C | 579 °F | Thallium | Tl | 81 |
| 594.18 K | 321.18 °C | 610.12 °F | Cadmium | Cd | 48 |
| 600.6 K | 327.6 °C | 621.7 °F | Lead | Pb | 82 |
| 692.73 K | 419.73 °C | 787.51 °F | Zinc | Zn | 30 |
| 722.65 K | 449.65 °C | 841.37 °F | Tellurium | Te | 52 |
| 903.9 K | 630.9 °C | 1167.6 °F | Antimony | Sb | 51 |
| 913 K | 640 °C | 1184 °F | Plutonium | Pu | 94 |
| 913 K | 640 °C | 1184 °F | Neptunium | Np | 93 |
| 922 K | 649 °C | 1200 °F | Magnesium | Mg | 12 |
| 933.25 K | 660.25 °C | 1220.45 °F | Aluminum | Al | 13 |
| 973 K | 700 °C | 1292 °F | Radium | Ra | 88 |
| 1002 K | 729 °C | 1344 °F | Barium | Ba | 56 |
| 1042 K | 769 °C | 1416 °F | Strontium | Sr | 38 |
| 1071 K | 798 °C | 1468 °F | Cerium | Ce | 58 |
| 1081 K | 808 °C | 1486 °F | Arsenic | As | 33 |
| 1095 K | 822 °C | 1512 °F | Europium | Eu | 63 |
| 1097 K | 824 °C | 1515 °F | Ytterbium | Yb | 70 |
| 1112 K | 839 °C | 1542 °F | Calcium | Ca | 20 |
| 1133 K | 860 °C | 1580 °F | Einsteinium | Es | 99 |
| 1173 K | 900 °C | 1652 °F | Californium | Cf | 98 |
| 1193 K | 920 °C | 1688 °F | Lanthanum | La | 57 |
| 1204 K | 931 °C | 1708 °F | Promethium | Pm | 61 |
| 1204 K | 931 °C | 1708 °F | Praseodymium | Pr | 59 |
| 1210.4 K | 937.4 °C | 1719.3 °F | Germanium | Ge | 32 |
| 1234 K | 961 °C | 1762 °F | Silver | Ag | 47 |
| 1259 K | 986 °C | 1807 °F | Berkelium | B K | 97 |
| 1267 K | 994 °C | 1821 °F | Americium | Am | 95 |
| 1289 K | 1016 °C | 1861 °F | Neodymium | Nd | 60 |
| 1323 K | 1050 °C | 1922 °F | Actinium | Ac | 89 |
| 1337.58 K | 1064.58 °C | 1948.24 °F | Gold | Au | 79 |
| 1340 K | 1067 °C | 1953 °F | Curium | Cm | 96 |
| 1345 K | 1072 °C | 1962 °F | Samarium | Sm | 62 |
| 1357.6 K | 1084.6 °C | 1984.3 °F | Copper | Cu | 29 |
| 1405 K | 1132 °C | 2070 °F | Uranium | U | 92 |
| 1517 K | 1244 °C | 2271 °F | Manganese | Mn | 25 |
| 1551 K | 1278 °C | 2332 °F | Beryllium | Be | 4 |
| 1585 K | 1312 °C | 2394 °F | Gadolinium | Gd | 64 |
| 1630 K | 1357 °C | 2475 °F | Terbium | Tb | 65 |
| 1683 K | 1410 °C | 2570 °F | Silicon | Si | 14 |
| 1685 K | 1412 °C | 2574 °F | Dysprosium | Dy | 66 |
| 1726 K | 1453 °C | 2647 °F | Nickel | Ni | 28 |
| 1743 K | 1470 °C | 2678 °F | Holmium | Ho | 67 |
| 1768 K | 1495 °C | 2723 °F | Cobalt | Co | 27 |
| 1795 K | 1522 °C | 2772 °F | Erbium | Er | 68 |
| 1799 K | 1526 °C | 2779 °F | Yttrium | Y | 39 |
| 1808 K | 1535 °C | 2795 °F | Iron | Fe | 26 |
| 1812 K | 1539 °C | 2802 °F | Scandium | Sc | 21 |
| 1818 K | 1545 °C | 2813 °F | Thulium | Tm | 69 |
| 1825 K | 1552 °C | 2826 °F | Palladium | Pd | 46 |
| 1933 K | 1660 °C | 3020 °F | Titanium | Ti | 22 |
| 1936 K | 1663 °C | 3025 °F | Lutetium | Lu | 71 |
| 2028 K | 1755 °C | 3191 °F | Thorium | Th | 90 |
| 2045 K | 1772 °C | 3222 °F | Platinum | Pt | 78 |
| 2113 K | 1600 °C | 2912 °F | Protactinium | Pa | 91 |
| 2125 K | 1852 °C | 3366 °F | Zirconium | Zr | 40 |
| 2130 K | 1857 °C | 3375 °F | Chromium | Cr | 24 |
| 2175 K | 1902 °C | 3456 °F | Vanadium | V | 23 |
| 2239 K | 1966 °C | 3571 °F | Rhodium | Rh | 45 |
| 2473 K | 2200 °C | 3992 °F | Technetium | Tc | 43 |
| 2500 K | 2227 °C | 4041 °F | Hafnium | HF | 72 |
| 2523 K | 2250 °C | 4082 °F | Ruthenium | Ru | 44 |
| 2573 K | 2300 °C | 4172 °F | Boron | B | 5 |
| 2716 K | 2443 °C | 4429 °F | Iridium | Ir | 77 |
| 2741 K | 2468 °C | 4474 °F | Niobium | Nb | 41 |
| 2890 K | 2617 °C | 4743 °F | Molybdenum | Mo | 42 |
| 3269 K | 2996 °C | 5425 °F | Tantalum | Ta | 73 |
| 3300 K | 3027 °C | 5481 °F | Osmium | Os | 76 |
| 3453 K | 3180 °C | 5756 °F | Rhenium | Re | 75 |
| 3680 K | 3407 °C | 6165 °F | Tungsten | W | 74 |
| 3773 K | 3500 °C | 6332 °F | Carbon | C | 6 |